3-(Methacryloyloxy)propyltrimethoxysilane CAS NO.2530-85-0
- FOB Price: USD: 1.00-1.00 /Metric Ton Get Latest Price
- Min.Order: 1 Kilogram
- Payment Terms: L/C,T/T
- Available Specifications:
99%(1-5)Metric Ton99%(5-20)Metric Ton
- Product Details
Keywords
- 3-(Methacryloyloxy)propyltrimethoxysilane
- γ-methacryloxypropyltrimethoxysilane
- CAS: 2530-85-0
Quick Details
- ProName: 3-(Methacryloyloxy)propyltrimethoxysil...
- CasNo: 2530-85-0
- Molecular Formula: C10H22O4Si
- Appearance: Colorless clear liquid
- Application: wetting agent
- DeliveryTime: Within 2 weeks after order confirmatio...
- PackAge: 25kg/drum
- Port: Qingdao Port
- ProductionCapacity: 2000 Metric Ton/Year
- Purity: 99%
- Storage: Preserve in well-closed, light-resista...
- Transportation: By sea
- LimitNum: 1 Kilogram
- CAS: 2530-85-0
Superiority
Chemical Name: γ- methacryloxypropyl trimethoxy silane
The main chemical components: CH2C (CH3) COO (CH2)3Si (OCH3)3
Molecular weight: 248.4g/mol
It is soluble in methanol, ethanol, isopropanol, acetone, benzene, toluene and xylene. After hydrolysis, it can be dissolved in water with pH 4.0 under stirring. After hydrolysis, methanol is produced.
Application areas:
Plastic products, rubber products, paints, inks, composite materials, magnetic materials, adhesives, casting, synthetic amino silicone oil, etc.
Application object:
1. Resins: phenolic, urea-formaldehyde, furan, nylon, polyurethane, unsaturated polyester, alkyd resin, acrylic resin and natural rubber, styrene-butadiene rubber, neoprene rubber, nitrile rubber, EPDM, PE, PP, PVC, S BS, etc.
2. Fillers: quartz, talc, kaolin, mica, white carbon black, wollastonite, glass fiber, Al(OH)3, Mg(OH)2, metals and their oxides, etc.
Product Features:
1. Treating the glass fiber yarn with a wetting agent (containing film-forming agent, lubricant and antistatic agent) containing the silane coupling agent KH-570 can improve the mechanical strength of this glass fiber yarn-reinforced composite material.
2. Improve the dry and wet mechanical strength of polyester composites filled with silica, glass, silicate and metal oxides.
3. Improve the wet electrical properties of many inorganic mineral filled composite materials such as cross-linked ethylene and polyvinyl chloride.
4. It can be copolymerized with vinyl acetate and acrylate or methacrylate monomers to make a moisture-curable silylated polymer. These silylated polymers are widely used in coatings, adhesives and sealants to provide excellent adhesion and durability.
Details
Appearance | colorless transparent liquid |
Flash point Tag sealed cup (ASTM D93): | 108℃ |
Density: ρ (25℃) | 1.045 |
Boiling point (760mmHg) | 255℃ |
Refractive index N D 25℃ | 1.429 |